V96ts (1960)
For the manufacture of loaded power parts and structures.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 4784-97 | < 0.4 | < 0.3 | 2.3–3 | < 0.1 | < 0.03 | 2–2.6 | 8–9 | 0.1–0.2 | 84.27–87.6 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Analogues
| USA |
|---|
| AA7049 |
Standards
| Standard | Description |
|---|---|
| OST 1 90048-90 | |
| TU 1-804-106-2012 | |
| TU 1-804-088-2012 | |
| GOST 4784-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |