VAD1B
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Be, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Zr, % |
Al, % |
OE, % |
ET, % |
| GOST 17232-99 |
< 0.3 |
< 0.2 |
0.0002–0.005 |
2.3–2.7 |
0.35–0.8 |
0.03–0.1 |
3.8–4.5 |
< 0.1 |
0.07–0.2 |
90.945–93.4498 |
< 0.05 |
< 0.1 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| OE |
% |
Other items |
| Si |
% |
Silicon |
| Be |
% |
Beryllium |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |