VAL5
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Foundry aluminum alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Be, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Zr, % |
Al, % |
Примеси, % |
| GOST 2685-75 |
< 0.6 |
6.5–8.5 |
< 0.1 |
0.15–0.4 |
0.35–0.55 |
< 0.1 |
0.1–0.3 |
< 0.3 |
< 0.3 |
< 0.2 |
87.65–92.9 |
< 1 |
Information on suppliers
Analogues
| Germany |
European Union |
USA |
| G-AlSi7Mg wa DIN 1725 Part 2 |
AS7G 03 |
EN AC-42100 ASME SB/EN 1706 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Be |
% |
Beryllium |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |