VBr3
Production of castings-blanks-duty methods of centrifugal casting, permanent mold casting in a stationary manner, and pulling from a melt.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Tinless cast bronze |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Sb, % | Al, % | Pb, % | As, % | P, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 493-79 | 1.2–1.6 | 0.6–0.6 | < 0.002 | 0.4–1 | 0.8–1.3 | 0.5–1 | 72.5–76.97 | 16–18 | < 0.005 | 3–3.5 | < 0.002 | < 0.01 | < 0.002 | < 0.01 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 493-79 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |
| S | % | Sulfur |