VDS-75
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Nickel alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mg, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | La, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 1 | < 0.4 | < 0.02 | < 0.03 | < 0.4 | 14.1–17 | 7.5–9 | 2–2.7 | < 0.07 | 49.335–60.4 | < 0.2 | 4.6–5.1 | < 0.03 | < 0.015 | 0.1–0.16 | < 0.01 | 1–2 | < 0.03 | 0.8–1.5 | 9.5–11 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| La | % | Lanthanum |
| Mo | % | Molybdenum |
| W | % | Tungsten |