VZHL1 (VZhL1-VI)
Production of cast bar stock for further refining during casting of blades and other shaped castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1-90126 - 85 | 6–7.5 | 1.2–2 | 0.09–0.13 | < 0.3 | 15–17 | 2–3 | 59.56–68.11 | 2–2.8 | < 0.02 | 0.1–0.17 | < 0.02 | 3.5–5 | 2–2.5 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| Workpiece | OST 1-90126 - 85 | 670 |
Brinell hardness number
Standards
| Standard | Description |
|---|---|
| OST 1-90126 - 85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |