VZHL14
Fabrication of blanks intended for further refining the production of shaped castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | Ce, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 1-92-160 - 90 | 8–10 | < 0.4 | < 0.005 | < 0.4 | 18–20 | 2.6–2.9 | 59.175–65.65 | 1.2–1.5 | < 0.02 | < 0.01 | 0.05–0.08 | < 0.01 | 4.5–5.5 |