VZHL2 (VLL2-VI)
Production of cast bar stock for further refining during casting of blades and other shaped castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1-90126 - 85 | 2–3.5 | 1–2 | < 0.065 | 12–15 | 2–3.2 | 48.025–61.39 | 1.5–3 | < 0.02 | 0.11–0.17 | < 0.02 | 12–15 | 8–10 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 1-90126 - 85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |