VH4L-VI
High-temperature alloys casting vacuum melting.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Ca, % | Cr, % | Ti, % | Ni, % | Al, % | Ce, % | C, % | S, % | Nb, % | Y, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1 90126-85 | < 0.5 | < 0.3 | < 0.008 | < 0.02 | 32–35 | 0.7–1.3 | 56.232–63.57 | 0.7–1.3 | < 0.03 | 0.03–0.1 | < 0.01 | 0.7–1.3 | < 0.4 | 2.3–3.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 1 90126-85 | OST 1 90126-85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Ca | % | Calcium |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Ce | % | Cerium |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Y | % | Yttrium |
| Mo | % | Molybdenum |