VK10-HOM (VK10HOM)
For the processing of materials by cutting: drilling, core drilling, reaming, milling and gear milling steel, cast iron, certain hard materials and non-metals in solid, small-sized tool.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Hard sintered alloys |
Chemical composition
| Standard | WC, % | TaC, % | Co, % |
|---|---|---|---|
| GOST 3882-74 | > 88 | < 2 | < 10 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 14.3–14.7 |
Standards
| Standard | Description |
|---|---|
| GOST 3882-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| TaC | % | Tantalum carbide |
| WC | % | Wolfram carbide |
| Co | % | Cobalt |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |