VK6-OM (VK6OM)
For the processing of materials by cutting: finishing and semi-finishing of hard alloyed and chilled cast iron, hardened steel and certain grades of stainless high-strength and heat-resistant steels and alloys, especially titanium-based alloys, tungsten and molybdenum (turning, boring, reaming, tapping, scraping).
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Hard sintered alloys |
Chemical composition
| Standard | WC, % | Co, % |
|---|---|---|
| GOST 3882-74 | > 94 | < 6 |
Information on suppliers
Analogues
| Germany |
|---|
| HG012 |
Standards
| Standard | Description |
|---|---|
| GOST 3882-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| WC | % | Wolfram carbide |
| Co | % | Cobalt |