VKNA-25
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Nickel alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Al, % | Ce, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 6–7.5 | 1.2–2 | 0.09–0.13 | < 0.3 | < 0.05 | 15–17 | 2–3 | 59.5–68.11 | 2–2.8 | < 0.01 | < 0.02 | 0.1–0.17 | < 0.02 | 3.5–5 | 2–2.5 |
Information on suppliers
Analogues
| Russia |
|---|
| ВЖЛ1-ВИ ОСТ 1 90126-85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |