VN-4
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Niobium |
Chemical composition
| Standard | Zr, % | C, % | Nb, % | Mo, % |
|---|---|---|---|---|
| 1–2 | 0.25–0.4 | 87.1–90.25 | 8.5–10.5 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Zr | % | Zirconium |
| C | % | Carbon |
| Nb | % | Niobium |
| Mo | % | Molybdenum |