VNM3-2
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Tungsten |
Chemical composition
| Standard | Cu, % | Ni, % | W, % |
|---|---|---|---|
| 1.6–2.1 | 2.9–3.4 | 94.5–95.5 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Cu | % | Copper |
| Ni | % | Nickel |
| W | % | Tungsten |