VPr2 (Vpr-2)
Solder for the soldering of parts and components of high-temperature alloys and stainless steels
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cu, % | Ni, % | Li, % |
|---|---|---|---|---|---|---|
| OST 1 90082-88 | 0.6–1.2 | 0.1–0.5 | 22–26 | 66.05–72.15 | 5–6 | 0.15–0.25 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 1 90082-88 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |
| Li | % | Li |