VPr4 (Vpr-4)
Solder for the soldering of parts and components of high-temperature alloys and stainless steels
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper Alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cu, % | Ni, % | P, % |
|---|---|---|---|---|---|---|---|---|
| OST 1 90082-88 | 1–1.5 | 0.8–1.2 | 0.15–0.25 | 27–30 | 4–6 | 30.85–38.95 | 28–30 | 0.1–0.2 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 1 90082-88 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |