BP-27VP
Tungsten-rhenium alloy. High heat resistance, durability and corrosion resistance to aggressive gas and liquid environments.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Rhenium, alloys with rhenium |
Chemical composition
| Standard | W, % | Re, % |
|---|---|---|
| TU 48-19-274-77 | 73 | 27 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| W | % | Tungsten |
| Re | % | Rhenium |