VRN
Tungsten brand VRN. This brand of tungsten does not contain additives, but it allowed the presence of impurities in increased volume.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Refractory metals, carbide |
Tungsten |
Chemical composition
| Standard |
Fe, % |
Si, % |
Ca, % |
Al, % |
Mo, % |
W, % |
| GOST 19671-91 |
< 0.01 |
0.001–0.01 |
< 0.02 |
0.001–0.01 |
< 0.04 |
> 99.9 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
19300 |
55 |
Brinell hardness number
Casting and technological parameters
| melting point, °C |
Boiling temperature, °C |
| 3380 |
5555 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Ca |
% |
Calcium |
| Al |
% |
Aluminium |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |
| Boiling temperature |
°C |
The boiling point, boiling point is the temperature at which the liquid under constant pressure boils. |