VT1-00sv
Melting point: 1668 ° C.
For the manufacture of welding wire
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Titanium, titanium alloys | Technical Titan |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Al, % | C, % | O, % | N, % | H, % |
|---|---|---|---|---|---|---|---|---|
| GOST 27266-87 | < 0.15 | < 0.08 | 99.39–99.9 | < 0.2 | < 0.05 | < 0.12 | < 0.03 | < 0.003 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|
| Wire | GOST 27265-87 | 295 | 30 |
Standards
| Standard | Description |
|---|---|
| GOST 27266-87 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ti | % | Titan |
| Al | % | Aluminium |
| C | % | Carbon |
| O | % | Oxygen |
| N | % | Nitrogen |
| H | % | Hydrogen |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |