VT1L
for the manufacture of castings
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Titanium, titanium alloys |
Foundry titanium alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Ti, % |
C, % |
O, % |
N, % |
W, % |
H, % |
|
< 0.3 |
< 0.15 |
98.635–99.7 |
< 0.15 |
< 0.2 |
< 0.05 |
< 0.2 |
< 0.015 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
|
|
|
|
|
350 |
10 |
|
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Ti |
% |
Titan |
| C |
% |
Carbon |
| O |
% |
Oxygen |
| N |
% |
Nitrogen |
| W |
% |
Tungsten |
| H |
% |
Hydrogen |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |