VT20L
for the manufacture of castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Titanium, titanium alloys | Foundry titanium alloys |
Chemical composition
| Standard | Ti, % | V, % | Zr, % | Al, % | Mo, % |
|---|---|---|---|---|---|
| OST 1-90060-92 | 86.2–91.7 | 0.8–1.8 | 1.5–2.5 | 5.5–7.5 | 0.5–2 |
Information on suppliers
Mechanical properties at 20 °C
Standards
| Standard | Description |
|---|---|
| OST 1-90060-92 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Ti | % | Titan |
| V | % | Vanadium |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| Mo | % | Molybdenum |