VT25U
Heat resistant alloy
Discs and blades of gas turbine engine compressors with operating temperatures up to 550 degrees., Long service life
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Titanium, titanium alloys | Wrought Titanium Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Ti, % | Zr, % | Al, % | C, % | O, % | Mo, % | N, % | W, % | H, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1-90013-81 | < 0.15 | 0.1–0.3 | 1–2.5 | 78.95–85.7 | 3.5–4.5 | 6–7 | < 0.1 | < 0.15 | 3.5–4.5 | < 0.04 | 0.4–1.5 | < 0.01 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 1-90013-81 |