VT6L
for the manufacture of castings
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Titanium, titanium alloys |
Foundry titanium alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Ti, % |
V, % |
Zr, % |
Al, % |
C, % |
O, % |
N, % |
W, % |
H, % |
| OST 1-90060-92 |
< 0.3 |
< 0.15 |
87.435–91.5 |
3.5–4.5 |
< 0.3 |
5–6.5 |
< 0.1 |
< 0.15 |
< 0.05 |
< 0.2 |
< 0.015 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
| 20 |
115 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
|
|
|
|
|
880 |
4 |
300 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Ti |
% |
Titan |
| V |
% |
Vanadium |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |
| C |
% |
Carbon |
| O |
% |
Oxygen |
| N |
% |
Nitrogen |
| W |
% |
Tungsten |
| H |
% |
Hydrogen |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |