VT8
It is used in GTE parts (disks, blades of a low pressure compressor, fan mounting details). Maximum operating temperature is up to 480 degrees C
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Titanium, titanium alloys |
Wrought Titanium Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Ti, % |
Zr, % |
Al, % |
C, % |
O, % |
Mo, % |
N, % |
H, % |
| GOST 19807-91 |
< 0.3 |
0.2–0.4 |
88.485–91.2 |
< 0.5 |
5.8–7 |
< 0.1 |
< 0.15 |
2.8–3 |
< 0.05 |
< 0.015 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
4520 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\psi$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
d5, % |
Treatment |
| Rod |
GOST 26492-85 |
|
|
|
930–980 |
15–20 |
200–300 |
6–8 |
|
| Rod |
GOST 19807-91 |
|
|
enhanced quality |
930–1230 |
19–30 |
300 |
7–9 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Ti |
% |
Titan |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |
| C |
% |
Carbon |
| O |
% |
Oxygen |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
| H |
% |
Hydrogen |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| d5 |
% |
Elongation at break |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\psi$$ |
% |
Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |