VZH13
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Nickel, nickel alloys |
Nickel alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Zr, % |
Ce, % |
P, % |
C, % |
S, % |
Nb, % |
La, % |
Mo, % |
|
< 2.5 |
< 0.4 |
< 0.03 |
< 0.4 |
15.5–17.5 |
0.8–1.2 |
< 0.07 |
70.588–77.68 |
< 0.005 |
< 0.01 |
< 0.01 |
0.02–0.07 |
< 0.007 |
2.2–2.6 |
< 0.01 |
3.8–4.6 |
Information on suppliers
Analogues
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Zr |
% |
Zirconium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| La |
% |
Lanthanum |
| Mo |
% |
Molybdenum |