VZHL1-VI
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Heat resistant steels and alloys |
Heat resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| OST 1 90126-85 |
6–7.5 |
1.2–2 |
0.09–0.13 |
< 0.3 |
< 0.05 |
15–17 |
2–3 |
59.5–68.11 |
2–2.8 |
< 0.01 |
< 0.02 |
0.1–0.17 |
< 0.02 |
3.5–5 |
2–2.5 |
Information on suppliers
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |