VZHM4-VI
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Co, % | Cr, % | Ni, % | Al, % | P, % | La, % | Mo, % | W, % | Ru, % | Re, % | Ta, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 6.7 | 4.7 | 36.7 | 0.7 | 13.3 | 9.3 | 7.7 | 1.5 | 4.7 | 3.3 | 10.2 |
Note: Typical chemical composition
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| La | % | Lanthanum |
| Mo | % | Molybdenum |
| W | % | Tungsten |
| Ru | % | Ruthenium |
| Re | % | Rhenium |
| Ta | % | Tantalum |