YUNDKBA
Cast hard magnetic alloy on iron-nickel-aluminum base. Magnetic anisotropy is available
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Magnetic Hard Precision Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Co, % | Ti, % | Cu, % | Ni, % | Al, % | Nb, % |
|---|---|---|---|---|---|---|---|---|
| GOST 17809-72 | 44.75–53 | < 0.6 | 24–26 | < 0.3 | 3–4.5 | 12.5–15 | 7.5–8.7 | < 0.15 |