ZHLSn20PbС
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tin, lead, babity | Tin-lead solder |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Zn, % | Sb, % | Al, % | Pb, % | As, % | Cd, % | Ag, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| < 0.02 | 19.5–20.5 | < 0.1 | < 0.05 | < 0.001 | 0.5–3 | < 0.001 | 76.292–80 | < 0.02 | < 0.001 | < 0.015 |
Note: Sb + Bi + Cu < 0.08
Information on suppliers
Analogues
| Germany | European Union | USA |
|---|---|---|
| L-PbSn20Sb3 DIN 1707 | S-Pb78Sn20Sb2 EN 29453 | J473 (No. 5B) SAE J473 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Zn | % | Zinc |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |
| Ag | % | Silver |