ZI112 (ANS-16)
Steel welding wire from steel grade SV-10Х16Н25М6АФ (ЗИ112)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Materials for welding and soldering | Steel welding wire |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-2416-78 | 44.457–53.71 | < 0.4 | 1–2 | 15–17 | 24–27 | 0.7–1 | < 0.1 | < 0.018 | 0.07–0.11 | < 0.015 | 5.5–7 | 0.02–0.9 |
Information on suppliers
Properties
| Property |
|---|
| Typical Characteristics Elastic Modulus (Young's Modulus): 185 GPa |
| Typical Specifications Density: 7.82 g / cm3 |
| Typical characteristics Linear expansion coefficient: 11.3 (10 ^ 6) / ° С |
| Typical Characteristics Thermal Conductivity at 20 ° C: 17.2 W / m * K |
Analogues
| Russia |
|---|
| Н-151 ТУ 14-1-2416-78 |
Standards
| Standard | Description |
|---|---|
| TU 14-1-2416-78 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| N | % | Nitrogen |