ZI25-VD (03N18K8M3TYU-VD)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-4090-86 |
68.15–70.95 |
< 0.15 |
< 0.1 |
8–8.5 |
< 0.25 |
0.2–0.35 |
17.5–18.5 |
0.05–0.15 |
< 0.01 |
< 0.03 |
< 0.01 |
3.3–3.8 |
Information on suppliers
Свойства
| Свойство |
| Вычисляемые свойства Плотность: 8.2 г/см3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |