ZI66
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| TU 14-3-1348-2005 |
60.545–67.5 |
< 0.4 |
1–2 |
16–18 |
< 0.3 |
13–15 |
< 0.2 |
< 0.015 |
< 0.02 |
< 0.02 |
2.5–3.3 |
< 0.2 |
Information on suppliers
Properties
| Property |
| Pipes according to TU 14-3-1348-2005 Temporary resistance:> 490 MPa |
| Pipes according to TU 14-3-1348-2005 Elongation:> 40% |
| Operational characteristics According to GOST R 54803-2011 Sheet Application temperature: -70 - 450 ° C |
| Operational characteristics According to GOST R 54803-2011 Forgings Application temperature: -70 - 450 ° C |
| Operational characteristics According to GOST R 54803-2011 Long products Application temperature: -70 - 450 ° C |
| According to STO 00220227-006-2010 Application temperature: -70 - 450 ° C |
| According to the requirements of the Russian Maritime Register of Shipping Application temperature: -165 - 600 ° C |
| According to the requirements of the Russian Maritime Register of Shipping Steel class: A-6 |
| Calculated Properties Density: 7.96 g / cm3 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |