ZI90-VI (X12N8K5M2TU)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Co, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| 67.9–73.55 | 5–6 | 11.5–12.5 | 0.8–1.2 | 7–9 | 0.15–0.35 | < 0.01 | < 0.03 | < 0.01 | 2–3 |
Information on suppliers
Properties
| Property |
|---|
| Typical Characteristics Yield Strength: 1600 MPa |
| Typical Characteristics Temporary Resistance: 1700 MPa |
| Typical Characteristics Elongation: 10% |
| Typical Characteristics HRC Hardness: 48 |
| Typical characteristics Impact strength KCU at 20 ° C: 50 J / cm2 |
| Typical Characteristics Relative contraction: 55% |
| Calculated Properties Density: 7.94 g / cm3 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |