ZIO-8
Metal covered electrodes for special purpose manual arc welding austenitic steel.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| OST 5Р.9370-2011 | 55.13–64.5 | < 1 | 1–2.7 | 23–27 | 11.5–14 | < 0.02 | < 0.12 | < 0.03 |
Note: Deposited metal By agreement: S < 0.015, P < 0.020, Co < 0.050, Cu < 0.080. Al < 0.100