Zl 999,9
The alloy has high chemical resistance, but low mechanical properties. Color is bright yellow
For making jewelry, medals
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Gold jewelery |
Chemical composition
| Standard |
Bi, % |
Cu, % |
Sb, % |
Pb, % |
Au, % |
Примеси, % |
| GOST 30649-99 |
< 0.002 |
< 0.012 |
< 0.002 |
< 0.035 |
> 99.99 |
< 0.01 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
19300 |
Casting and technological parameters
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Примеси |
% |
Impurities |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| Au |
% |
Gold |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |