Zl 999,9m (ZlA-1)
For the production of ingots weighing from 1 to 1000, at intended for commercial and other purposes
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Au, % | Примеси, % |
|---|---|---|
| GOST Р 51572-2000 | > 99.9 | < 0.01 |
Note: All impurities: Cu + Zn + Si + Pb + Sn + Mg + Ni + Fe + Mn + Bi + Sb + Cr + Ag + Pt + Pd + Rh
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST Р 51572-2000 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Примеси | % | Impurities |
| Au | % | Gold |