Evil-1 (ZL999.9m)
For the production of gold ingots from 11,000 to 13,300 was supplied for the needs of the economy and exports. In coordination with the consumer manufacturing ingots other mass.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Mn, % | Cr, % | Cu, % | Zn, % | Ni, % | Sb, % | Pb, % | Ag, % | Au, % | Pt, % | Pd, % | Rh, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 28058-89 | < 0.001 | < 0.003 | < 0.001 | < 0.003 | < 0.001 | < 0.0005 | < 0.0005 | < 0.001 | < 0.001 | < 0.0005 | < 0.001 | < 0.001 | < 0.005 | < 99.99 | < 0.001 | < 0.003 | < 0.001 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 28058-89 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Pb | % | Lead |
| Ag | % | Silver |
| Au | % | Gold |
| Pt | % | Platinum |
| Pd | % | Palladium |
| Rh | % | Rhodium |