Evil-1P
For the production of gold ingots from 11,000 to 13,300 was supplied for the needs of the economy and exports. In coordination with the consumer mass production of other bars
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Mn, % | Cr, % | Cu, % | Zn, % | Ni, % | Sb, % | Pb, % | Ag, % | Au, % | Pt, % | Pd, % | Rh, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 28058-89 | < 0.0005 | < 0.001 | < 0.0005 | < 0.001 | < 0.0005 | < 0.0005 | < 0.0005 | < 0.0005 | < 0.0005 | < 0.0005 | < 0.0005 | < 0.0005 | < 0.005 | < 99.99 | < 0.0005 | < 0.0005 | < 0.0005 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 28058-89 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Pb | % | Lead |
| Ag | % | Silver |
| Au | % | Gold |
| Pt | % | Platinum |
| Pd | % | Palladium |
| Rh | % | Rhodium |