Evil 3
For the production of gold ingots from 11,000 to 13,300 was supplied for the needs of the economy and exports. In coordination with the consumer manufacturing ingots other mass.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Ag, % | Au, % | Pt, % | Pd, % | Rh, % |
|---|---|---|---|---|---|
| GOST 28058-89 | < 0.035 | < 99.95 | < 0.005 | < 0.01 | < 0.002 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 28058-89 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Ag | % | Silver |
| Au | % | Gold |
| Pt | % | Platinum |
| Pd | % | Palladium |
| Rh | % | Rhodium |