ZlM 91,6 (ZlM 916 GOST 6835-80)
Gold and alloys based on it.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Fe, % | Bi, % | Cu, % | Sb, % | Pb, % | Au, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| GOST 6835-2002 | < 0.15 | < 0.005 | < 8 | < 0.005 | < 0.005 | 91.3–91.9 | < 0.16 |