ZlM 980
Gold and gold alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Fe, % | Bi, % | Cu, % | Sb, % | Pb, % | Au, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| GOST 6835-80 | < 0.1 | < 0.005 | 1.7–2.7 | < 0.005 | < 0.005 | 97.3–98.3 | < 0.11 |
Information on suppliers
Analogues
| Russia |
|---|
| ЗлМ 98 |
Standards
| Standard | Description |
|---|---|
| GOST 6835-80 | GOST 6835-80 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Sb | % | Antimony |
| Pb | % | Lead |
| Au | % | Gold |