ZlN 95
Gold and alloys on its basis.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Fe, % | Bi, % | Ni, % | Sb, % | Pb, % | Au, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| GOST 6835-2002 | < 0.1 | < 0.005 | 4.275–5.275 | < 0.005 | < 0.005 | 94.5–95.5 | < 0.11 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 6835-2002 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Bi | % | Bismuth |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Pb | % | Lead |
| Au | % | Gold |