ZlPdPl 60-30-10
Gold and alloys on its basis.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Fe, % | Pb, % | Au, % | Pt, % | Pd, % | Ir, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| GOST 6835-2002 | < 0.03 | < 0.003 | 59.4–60.6 | 9.5–10.5 | 29.5–30.5 | < 0.15 | < 0.18 |
Note: Ir: Ir + Rh
Information on suppliers
Analogues
| Russia |
|---|
| ЗлПдПл-30-10 ГОСТ 6835-80 |
Standards
| Standard | Description |
|---|---|
| GOST 6835-2002 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Pb | % | Lead |
| Au | % | Gold |
| Pt | % | Platinum |
| Pd | % | Palladium |
| Ir | % | Iridium |