ZlSrKdM 750-30
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold, gold alloys |
Chemical composition
| Standard | Cu, % | Ag, % | Au, % | Pt, % |
|---|---|---|---|---|
| TU 48-1-255-87 | 8.7–11.4 | 2.5–3.5 | 74.7–75.3 | 11.4–12.5 |