ZlSrM 750-150 (ZlSrM 75-15)
The alloy is suitable for all types of cold working; For machining, it is preferable to use a welded or hardened state; during investment casting, the alloy should be melted in vacuum and poured under a protective atmosphere. Sample 750, color yellow. Melting point 890 — 920 ° C.
For making jewelry, souvenirs; alloy soldered well and is used for the manufacture of coated enamel
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold jewelery |
Chemical composition
| Standard | Fe, % | Bi, % | Cu, % | Sb, % | Pb, % | Ag, % | O, % | Au, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 30649-99 | < 0.15 | < 0.005 | 8.65–10.33 | < 0.005 | < 0.005 | 14.5–15.5 | < 0.007 | 75–75.5 | < 0.17 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 15530 |
Casting and technological parameters
| melting point, °C |
|---|
| 890–920 |
Standards
| Standard | Description |
|---|---|
| GOST 30649-99 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Sb | % | Antimony |
| Pb | % | Lead |
| Ag | % | Silver |
| O | % | Oxygen |
| Au | % | Gold |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
Description of the casting and technological parameters
| Parameter | Units of measurement | Description |
|---|---|---|
| melting point | °C | The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |