ZlSrM 950-25 (ZlSrM 95-2,5)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Gold jewelery |
Chemical composition
| Standard | Fe, % | Bi, % | Cu, % | Sb, % | Pb, % | Ag, % | Au, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|
| GOST 6835-80 | < 0.08 | < 0.003 | 2–2.8 | < 0.003 | < 0.003 | 2–3 | 94.7–95.3 | < 0.09 |