ZlSrPdKd585-280-100 (ZlSrPdKd 58.5-28-10)
The alloy is suitable for casting and cold working; ductile in the annealed condition; not subject to hot cracking during annealing or brazing. Sample 585, white color. Melting point 1160 — 1190 ° C.
For the manufacture of jewelry, souvenirs, smoking accessories
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Gold jewelery |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Sb, % |
Pb, % |
Cd, % |
Ag, % |
O, % |
Au, % |
Pd, % |
| GOST 30649-99 |
< 0.15 |
< 0.005 |
< 0.005 |
< 0.005 |
1.65–4.33 |
27.5–28.5 |
< 0.007 |
58.5–59 |
9.5–10.5 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
14600 |
Casting and technological parameters
| melting point, °C |
| 1160–1190 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Bi |
% |
Bismuth |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| Cd |
% |
Cadmium |
| Ag |
% |
Silver |
| O |
% |
Oxygen |
| Au |
% |
Gold |
| Pd |
% |
Palladium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |