D51500
Classification
| Country |
Section |
Category |
| USA |
Steels with specified mechanical properties |
Alloy Steels Casting |
Chemical composition
| Standard |
Fe, % |
P, % |
S, % |
| UNS |
> 99.96 |
< 0.02 |
< 0.02 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma_{Y}$$, $$MPa$$ |
Treatment |
|
|
|
|
|
> 1034 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| P |
% |
Phosphorus |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |