F10003
Classification
| Country | Section | Category |
|---|---|---|
| USA | Iron, including Ductile Irons and Cast Irons | Cast Iron, Gray |
Chemical composition
| Standard | Fe, % | C, % |
|---|---|---|
| UNS | > 97.2 | < 2.8 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| C | % | Carbon |