F10006
Classification
| Country | Section | Category |
|---|---|---|
| USA | Iron, including Ductile Irons and Cast Irons | Cast Iron, Gray |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|
| UNS | 93.1–94.4 | 1.9–2.3 | 0.6–0.9 | < 0.15 | 3.1–3.4 | < 0.15 |